Effect of Sintering Temperature and Time on Microstructure and Properties of Cobalt-based Alloys
Author of the article:LV Songtao;SU Yixiang;YIN Zhangxuan;CUI Yanping;LIANG Tengwen;YANG Meimei
Author's Workplace:Department of Transportation,Zhengzhou Professional Technical Institute of Electronic & Information,Zhengzhou 451450,China;School of Materials Science and Engineering,Lanzhou University of Technology,Lanzhou 730050,China
Key Words:cobalt based alloy powder sintering temperature holding time
Abstract:
The effect of sintering temperature and holding times on microstructure and properties of cobalt-based alloy were investigated by OM and Brinell-Rockwell hardness tester. The results show that the optimal sintering temperature and holding time for cobalt-based alloy are 1 290 ℃ and 2.5~3 h, respectively, and cobalt-based alloy has the best microstructure and mechanical properties.